Skip to main content

FC - Application on Vinyl

Craftsman Guide / Preparation & Substrates Application: Vinyl Sheet. Practical guide for preparation, leveling transitions, and priming on vinyl sheeting in wet rooms.. 🛑 Before You Start — Inspect t…

tomas martinsson
Updated by tomas martinsson
Craftsman Guide / Preparation & Substrates

Application: Vinyl Sheet

Practical guide for preparation, leveling transitions, and priming on vinyl sheeting in wet rooms.

🛑 Before You Start — Inspect the Vinyl Sheet:
No Bubbles or Delamination: Inspect the entire vinyl membrane thoroughly. The sheet must be fully adhered and not lifting at corners or along wall upstands.
Critical Around Floor Drains: Ensure the sheet has not delaminated or compromised its bond around the floor drain. Any void or deflection under the membrane will cause the microcement to crack over time.
Sample Board: Always produce a sample of at least 60×60 cm in the correct color and texture for client approval.
💡 Tips for Corners and Finish on Vinyl Sheeting:
• Vinyl sheets often have overlaps and coved corners, making it harder to obtain angles as crisp as those on plasterboard or tiles.
Vinyl on Both Wall and Floor: Naturally results in rounded transitions. For sharper definition, tape and slice internal corners straight on the final coat.
Tile on Wall and Vinyl on Floor: Leveling the step at the vinyl upstand automatically straightens and squares the corner.

1. Leveling Transitions & Floor Drains

Upstands & Level Differences (Tile on Wall / Vinyl on Floor)

Prime the vinyl upstand on the wall with a bonding primer designed for non-porous substrates (e.g., Monogrip). Then flush the transition flush using cement-based repair mortar or tile adhesive. Alternatively, install a thin wet-room board to meet the tile edge flush.

Floor Drains & Grates

New Low-Profile Grate: To avoid a plastic cover resting on and wearing against the surface layer, a low-profile microcement grate (e.g., Purus Sun) or mosaic grate is recommended. Bond the frame with sealing adhesive and skim flush with repair mortar prior to applying microcement.
Existing Cover: If retaining the original clamping ring, apply primer, reinforcement mesh, and microcement right down to the perimeter edge of the clamping ring.

2. Priming Vinyl Sheet

Floor: Forprime DPM

2-component epoxy primer for non-porous floor membranes.

Application: Roll Forprime DPM evenly across the entire vinyl floor.
Sand Blinding: Always blind to saturation with quartz sand if the next coat is Microbase XT. Prior to Forprime HB/FL, sand blinding is only necessary if the coat is not applied within 24 hours.
Drying Time: Allow to cure for at least 6–8 hours before walking on the surface.
Wall: Monogrip

Grip primer with quartz texture for vertical surfaces.

Application: Roll a thin, even coat of Monogrip over the wall vinyl.
System Selection: Standard primer prior to build-up with Monostone XL and reinforcement mesh.
Drying Time: Allow to dry for approximately 30–60 minutes to a rough, non-tacky surface before skim-coating.
Drying Times & Ventilation: Ensure repair mortars and primers are completely dry before applying base coats. Maintain good ventilation in the workspace with open doors and circulating fans.