FC - Mixing and Pigmentation (ENG)
How to pigment and mix Microquartz, Microbase XT and Monostone. Always pigment a full bucket of component A at a time.
Mixing Instructions & Pigmentation
Instructions for pigmentation and mixing of Microquartz, Microbase XT, and Monostone.
Always pigment a full bucket of Component A at a time to ensure accurate color. Pigmenting the entire bucket does not mean all material must be applied immediately – measure out smaller batches as needed. Pigmenting smaller individual batches can lead to color variations between mixes (best reserved for the initial base coat).
Pigmentation for the 2-component products (Microquartz and Microbase XT) must be carried out at least 2 hours before application, but is ideally done the day before. Once Component A is pigmented, it can be stored for months prior to adding the hardener.
Step 1: Pigmenting Component A (Microquartz & Microbase XT)
- "1" shade (Microquartz): Approx. 100 g water (e.g. Feather 1).
- "2" shade (Microquartz): Approx. 150–200 g water (e.g. Feather 2, start around 150 g).
- "3" shade (Microquartz): Requires more water due to high pigment load. Add what is necessary to dissolve powder completely.
- Microbase XT: Add approx. 1.5 times more water than for Microquartz (approx. 150–300 g water).
Both Microbase XT and Microquartz Coarse carry very low risk when pigmented directly in the bucket. Pour water and pigment powder straight into Component A and mix thoroughly. Let the mixture rest for at least 2 hours before adding hardener. The coarser aggregates in these products significantly reduce the risk of pigment streaks.
Step 2: Adding Hardener (Component B)
• Microquartz: Mixed 916 : 84 (one 500 g bottle of Comp B to one 5.5 kg bucket of Comp A).
• Microbase XT: Mixed 92 : 8 (800 g Comp B to one 9.2 kg bucket of Comp A).
Step 3: Final Water Volume Prior to Application
Once the hardener has been added and mixed in, add the remaining water to achieve your desired working consistency.
You can always add more water, but you can never remove it. Start with a lower amount and increase gradually if needed. To ensure a uniform color across the entire area, use the exact same total water quantity in all buckets for the final coat.
Stated in grams of water per 1 kg of finished material (including water added during Step 1 pigmentation). Use the app for precise batch numbers:
| Product Type | Water per kg | Percentage (%) | Characteristics |
|---|---|---|---|
| Microbase XT | 20–80 g | 2–8 % | Base coat. Adapt water ratio to temperature and substrate. |
| Microquartz Smooth & Medium | 20–40 g | 2–4 % | Lower water ratio provides maximum hiding power / coverage. |
| Microquartz Coarse | 30–90 g | 4–9 % | Normally 5–6% on walls/smaller floors, 7–9% on larger floor areas. |
Pigmentation of Monostone (XL & L)
• Water amount: Add 50–200 g clean water to the pigment.
• Minimizing streak risk: Dissolve the pigment in water in a separate container before pouring it into the bucket to eliminate pigment specks and streaks.
• Mixing: Mix thoroughly with a paddle mixer until all pigment is evenly dispersed throughout the cement.
4. Next Steps
Choose a product guide for instructions on application, curing, and drying times:
How did we do?
FC - Forshield Topcoat & Sealer (ENG)
FC - Sanding Guide (ENG)